# Strange artifacts on angles

**URL:** <https://forum.sovol3d.com/t/strange-artifacts-on-angles/8539>\
**Category:** Sovol SV08\
**Created:** [August 15, 2025, 12:21pm UTC](https://forum.sovol3d.com/t/strange-artifacts-on-angles/8539 "2025-08-15T12:21:00Z")\
**Posts on this page:** 4\
**Page:** 1

<div class="post-metadata">

**Author:** ![vanix](https://avatars.discourse-cdn.com/v4/letter/v/7ab992/32.png) [@vanix](https://forum.sovol3d.com/u/vanix)\
**Post date:** [August 15, 2025, 12:21pm UTC](https://forum.sovol3d.com/t/strange-artifacts-on-angles/8539/1 "2025-08-15T12:21:00Z")

</div>

Anyone know how to fix thats artifacts. The belts are tensioned with a frequency of 110 hz, after that I calibrated the shapers, but the problem remains.

photo published on google drive:

> **[sovol sv08 - Google Drive](https://drive.google.com/drive/folders/1IUB1LkG29wfD7boI-NN6goAfgo70pEn6?usp=sharing)**

---

<div class="post-metadata">

**Author:** ![mich0111](https://yyz2.discourse-cdn.com/flex030/user_avatar/forum.sovol3d.com/mich0111/32/1176_2.png) [@mich0111](https://forum.sovol3d.com/u/mich0111)\
**Post date:** [August 15, 2025, 2:38pm UTC](https://forum.sovol3d.com/t/strange-artifacts-on-angles/8539/2 "2025-08-15T14:38:27Z")

</div>

Hello,

There are other reasons that could explain the presence of artifacts, such as incorrect filament settings:

- The temperature is not set correctly.

- The maximum flowrate is set too high, which makes the slicer think that the filament can flow faster than it actually can.

- The maximum flowrate is not calibrated correctly.

- Moisture is present in the filament spool. Although this is unlikely for PLA, it can happen with matte or silky PLA.

I suggest adjusting these settings using the calibration functions in Orcaslicer.

---

<div class="post-metadata">

**Author:** ![vanix](https://avatars.discourse-cdn.com/v4/letter/v/7ab992/32.png) [@vanix](https://forum.sovol3d.com/u/vanix)\
**Post date:** [August 15, 2025, 3:00pm UTC](https://forum.sovol3d.com/t/strange-artifacts-on-angles/8539/3 "2025-08-15T15:00:47Z")

</div>

temperature is correct and max flowrate is 2 times lower than this filament can do on my bambu lab, moisture cant be because i use different filament and one after drying. But thanks

---

<div class="post-metadata">

**Author:** ![cardoc](https://yyz2.discourse-cdn.com/flex030/user_avatar/forum.sovol3d.com/cardoc/32/6926_2.png) [@cardoc](https://forum.sovol3d.com/u/cardoc)\
**Post date:** [August 16, 2025, 12:09am UTC](https://forum.sovol3d.com/t/strange-artifacts-on-angles/8539/4 "2025-08-16T00:09:30Z")

</div>

Run the pressure advance calibration. You can set a global value in printer.cfg but the best way is to run it for each different filament and put it in the filament profile in your slicer.

More info at [https://ellis3dp.com/Pressure\_Linear\_Advance\_Tool/](https://ellis3dp.com/Pressure_Linear_Advance_Tool/)

After you get it dialed in reduce your “square\_corner\_velocity” in printer.cfg