# Bad layers

**URL:** <https://forum.sovol3d.com/t/bad-layers/2559>\
**Category:** Sovol SV06 Fully Open Source 3D Printer\
**Created:** [May 13, 2023, 12:55pm UTC](https://forum.sovol3d.com/t/bad-layers/2559 "2023-05-13T12:55:17Z")\
**Posts on this page:** 3\
**Page:** 1

<div class="post-metadata">

**Author:** ![Ayjay](https://avatars.discourse-cdn.com/v4/letter/a/ecccb3/32.png) [@Ayjay](https://forum.sovol3d.com/u/Ayjay)\
**Post date:** [May 13, 2023, 12:55pm UTC](https://forum.sovol3d.com/t/bad-layers/2559/1 "2023-05-13T12:55:17Z")

</div>

Hello everybody,

I got my SVO6 in the end of January and since then i have this problem. My prints are looking like this when the lines are not straight. And the start of a layer is sometimes lacking of material.

 ![IMG_20230512_171155](https://canada1.discourse-cdn.com/flex030/uploads/sovolforum/original/2X/1/1cf4e427ddc3d2cde9ea90dc51c7fc35fee7c741.jpeg)  
It’s my first time printing with PETG. But I have the same problems withs PLA.

I lubed every bearing when i got the printer and adjusted the steps of every motor.  
I’m using Cura right now and tried different settings.  
I also worked with different belt tensions But nothing worked so far.

---

<div class="post-metadata">

**Author:** ![Ayjay](https://avatars.discourse-cdn.com/v4/letter/a/ecccb3/32.png) [@Ayjay](https://forum.sovol3d.com/u/Ayjay)\
**Post date:** [May 13, 2023, 12:57pm UTC](https://forum.sovol3d.com/t/bad-layers/2559/2 "2023-05-13T12:57:06Z")

</div>

![IMG_20230217_154524](https://canada1.discourse-cdn.com/flex030/uploads/sovolforum/original/2X/8/854546070bb6b745fbbb5b678cdf484b9689e6ea.jpeg)

That’s with PLA.

---

<div class="post-metadata">

**Author:** ![Lion](https://yyz2.discourse-cdn.com/flex030/user_avatar/forum.sovol3d.com/lion/32/5586_2.png) [@Lion](https://forum.sovol3d.com/u/Lion)\
**Post date:** [May 24, 2023, 10:22pm UTC](https://forum.sovol3d.com/t/bad-layers/2559/3 "2023-05-24T22:22:49Z")

</div>

It looks like under extrusion.  
Did you set the retraction distance to 0.5 & retraction speed to 40.0…??  
Also it could be cause by using too low of a nozzle temp.  
PLA: 210\*-215\*  
PETG: 235\*-240\*